Nickel alloys display high strength and excellent corrosion resistance, making it a great metal for use in highly corrosive environments and high temperature environments. Hamilton Precision Metals offers an array of high-performance nickel alloys that are engineered to withstand a variety of severe operating conditions.
Technical Data
TYPE |
HPM
Nickel
200 |
HPM
Nickel
201 |
HPM
Nickel
270 |
HPM
400
|
HPM
600
|
HPM
X-750
|
Precision
C
|
HPM
Ni 36
|
Moly
Perm-
Alloy |
Rodar
|
HPM
Ni 42
|
HPM
Ni 52
|
HPM
80/20 A
|
HPM
80/20 Al
|
Ni |
99.5 |
99.5 |
99.97 |
66.0 |
BAL |
73.0 |
42.0 |
36.0 |
80.0 |
29.0 |
41.0 |
50.5 |
BAL |
BAL |
C |
.06 |
.01 |
.02 |
.12 |
|
|
.04 |
.02 |
.12 |
.05 |
.02 |
|
.30 |
|
Mn |
.25 |
.20 |
|
.90 |
.40 |
.70 |
.40 |
.35 |
.50 |
.30 |
.40 |
|
.40 |
|
Fe |
.15 |
.15 |
|
1.35 |
8.5 |
6.75 |
48.5 |
63.2 |
16.3 |
53.5 |
BAL |
BAL |
.50 |
.20 |
Si |
.05 |
.05 |
|
.15 |
|
|
|
.30 |
.50 |
.30 |
.35 |
.20 |
.20 |
1.25 |
Cu |
.05 |
.05 |
|
31.5 |
|
.05 |
.05 |
|
|
|
|
|
|
|
others |
|
|
|
|
Cr 15.5
|
Cr 15.0
Al .80
Ti 2.50
Cb .85 |
Cr 5.4
Al .7
Ti 2.4
|
|
Mo 4.8
|
Co 17.0
|
|
|
Cr 19.5
|
Cr 19.5
|
Density LB/CU IN |
.321 |
.321 |
.321 |
.319 |
.306 |
.298 |
.293 |
.291 |
.315 |
.302 |
.293 |
.300 |
.304 |
.304 |
Thermal
Expansion
Coefficient X
10-6/° C |
13.3 |
13.3 |
13.3 |
13.9 |
14.2 |
12.6 |
10.1 |
1.05 |
12.7 |
4.9 |
6.0 |
10.0 |
13.4 |
13.4 |
Thermal
Conductivity
W/M x K @ 100° C |
67 |
74 |
79 |
22 |
15 |
12 |
13 |
10.5 |
35 |
17 |
11 |
14 |
15 |
15 |
Electrical
Resistivity
MICROHM - CM |
9.5 |
8.5 |
7.5 |
51 |
103 |
119 |
102 |
82 |
59 |
49 |
70 |
43 |
108 |
108 |
Mechanical Properties
NICKEL MECHANICAL PROPERTIES |
TYPE |
Condition |
Tensile PSI |
Yield 0.2% Offset PSI |
Elongation % IN 2 * |
HPM Nickel 200
 |
Annealed |
67,000 |
20,000 |
47 |
HPM Nickel 201 |
Annealed |
67,000 |
20,000 |
47 |
HPM Nickel 270 |
Annealed |
65,000 |
20,000 |
47 |
HPM 400 |
Annealed |
75,000 |
30,000 |
30 |
HPM 600 |
Annealed |
90,000 |
40,000 |
45 |
Cold Rolled |
170,000 |
160,000 |
2 |
HPM X-750 |
Annealed |
140,000 |
65,000 |
40 |
Precision C |
Cold Rolled |
130,000 |
120,000 |
6.5 |
CR and Aged |
200,000 |
180,000 |
7.0 |
HPM Ni 36 |
Annealed |
70,000 |
40,000 |
35 |
Cold Rolled |
130,000 |
125,000 |
2 |
Moly Permalloy |
Annealed |
90,000 |
75,000 |
30 |
Cold Rolled |
160,000 |
150,000 |
1 |
Rodar |
Annealed |
75,000 |
50,000 |
30 |
HPM Ni 42 |
Annealed |
72,000 |
40,000 |
35 |
Cold Rolled |
110,000 |
105,000 |
5 |
HPM Ni 52 |
Annealed |
75,000 |
30,000 |
30 |
Cold Rolled |
130,000 |
125,000 |
1 |
HPM 80/20 A |
Annealed |
105,000 |
50,000 |
35 |
HPM 80/20 Al |
Annealed |
105,000 |
50,000 |
35 |
Cold Rolled |
190,000 |
185,000 |
1 |
* These values may be adjusted by control of process variable - consult HPM for desired values.